Item |
Description |
|
Function |
Continuously lifts and removes tramp ferrous metal from a conveyor carrying hot bulk material |
|
Standard circuit limit |
NdFeB (N-grade): continuous material duty up to ~80°C |
|
Hot-duty circuit options |
Ferrite (up to 250–300°C), NdFeB H/SH/UH/EH (120–200°C), SmCo (250–350°C), Class H electromagnet (up to ~180°C coil zone, oil-cooled higher) |
|
Cleaning belt |
Standard rubber fails above ~80°C; EPDM, silicone, aramid or glass-fibre belts required for hot duty |
|
Bearings |
High-temperature grease, extended housings, optional PT100 probes |
|
Typical applications |
Clinker and cement raw mix, sinter and coke handling, calcined lime, foundry returned sand, dried biomass, hot slag and DRI lines |
|
Key benefit |
Protects crusher wear parts and liners and downstream mills from destructive steel tramp iron even when the material is too hot for a standard unit |
Direct answer: In iron removal practice, "hot material" means a conveyed burden whose surface temperature at the magnet position exceeds roughly 80°C — the continuous operating ceiling of standard neodymium circuits and of ordinary rubber cleaning belts.
A surprising number of mining and minerals flows sit above that line for at least part of the time:
The number that matters is not the nameplate process temperature. It is the surface temperature of the burden directly beneath the magnet face, measured across a full shift including start-up spikes, because heat reaches the separator by radiation and by conduction through the iron it captures — not just through the air. For context on how magnetic iron removal fits into the wider plant flow, see the site's overview of magnetic separation equipment and the full range of industrial magnetic separators.
Direct answer: Because 80°C is the continuous operating limit of the standard (N-grade) neodymium magnet material used in most self-cleaning separators. Above it, field strength decays — first reversibly, then permanently.
All permanent magnets have a negative temperature coefficient. For neodymium, each 1°C rise reduces magnetic output by roughly 0.11–0.13%. Two consequences follow:
A single afternoon of overheating can therefore write off a magnet circuit — even though the unit looks perfectly normal the next morning.
Direct answer: A self-cleaning magnetic separator removes iron from material above 80°C when — and only when — its magnetic circuit, belt, bearings and shielding are chosen for the actual measured temperature, not the catalogue default.
Three habits separate plants that get years of protection from plants that quietly feed steel into their crushers. First, measure the burden temperature at the magnet position and treat the peak, not the average, as the design point. Second, remember that the magnet is only one link in a thermal chain: belts, grease, chains and scrapers usually fail first and cheaply if specified correctly. Third, keep a gauss map and a temperature log so decay shows up on a dashboard before it shows up as a broken jaw plate. For a duty above 150°C, ferrite or cooled electromagnetic circuits are the proven routes; between 80°C and 200°C, high-coercivity NdFeB with a heat shield gives the best balance of capture depth and cost. If you share your belt width, tonnage and measured temperature profile, a competent supplier will size the circuit and hand you the derated performance curve — ask for it before you buy.
Related Products
Related Technical Guides
Related Buyer Guides
Related Comparison Articles
Contact: Annie Lu
Email: annie.lu@huataogroup.com
Phone / WhatsApp: +86 180 3242 2676
Website: http://www.tufflexscreen.com
We warmly welcome customers from around the world to contact us and establish mutually beneficial partnerships.
Contact: Annie Lu
Tel: +86 18032422676
E-mail: manager11@huataogroup.com
Address: Zhonghua North Street, Shijiazhuang, Hebei, China