Huatao Group-Vibrating Screen Technology Solution and Service for Quarry & Mining Industry Since 2008.
Answer
If iron remains in the non-magnetic product, the cause may be an unsuitable magnetic field, poor feed distribution, insufficient particle liberation, excessive feed loading or iron impurities that are too weakly magnetic for the installed equipment. 🔧
1. The magnetic field is unsuitable. A low-intensity separator may capture magnetite effectively but leave some weakly magnetic minerals behind. Consider testing a high-intensity or high-gradient system if mineralogical analysis supports this choice.
2. The feed layer is too thick. Particles buried within a deep material bed may not experience sufficient magnetic force. Reduce loading or improve feed distribution and evaluate the change in iron removal.
3. The feed contains mixed particle sizes. Fine iron-bearing particles may behave differently from coarse particles. Screening or classification may improve consistency in some applications.
4. The target minerals are not liberated. Iron-bearing minerals locked inside larger composite particles may not separate cleanly until suitable grinding or other preparation is performed.
5. Operating conditions have changed. Check feed rate, moisture, drum speed, slurry flow and the condition of the magnetic assembly.
These factors are recognized considerations in magnetic separator design and mineral-processing optimization.
Take representative feed and product samples. Measure their iron content using the same analytical method, and record the feed rate and operating settings. If possible, examine the mineralogy of the remaining iron-bearing particles.
For example, if a silica sand plant captures visible magnetite but still fails its iron specification, the remaining impurity may be weakly magnetic hematite, iron-bearing mica or iron coatings on quartz grains. Simply increasing the magnet strength may not solve every case.
The best adjustment should be supported by testing and should improve product quality without causing unacceptable material loss or throughput reduction.