loading

Huatao Group-Vibrating Screen Technology Solution and Service for Quarry & Mining Industry Since 2008.

Custom Cut Polyurethane Skirting: What Actually Fits

Custom Cut Polyurethane Skirting: What Actually Fits

Quick Answer

Polyurethane skirting is routinely cut to order, and on most transfer points it should be. The strip is cut to belt width, bevelled to the trough angle measured at the idler set, squared to the skirtboard run and drilled to the clamp bar pitch. Off-the-shelf strip only works when a standard width and a 35-degree trough happen to match the conveyor already installed — which is less often than the catalogue implies.

Key Takeaways

✔ A bevelled cut matched to the measured trough angle separates a sealing skirt from a leaking one.

✔ Trough angle must be measured at the idler set, because replaced idler sets routinely change it.

✔ The working gap is contact at the centre and both wing transitions, 2 mm to 3 mm elsewhere.

✔ Custom cutting adds one to three weeks and cannot fix a worn, cambered or mis-tracked belt.

✔ Polyurethane holds a machined edge; rubber conforms to an imperfect belt.

✔ Ten to fifteen millimetres of take-up converts a replacement into an adjustment.

Summary Table

Item

Description

Function

Seals the gap between skirtboard and belt at loading and transfer points

Material

Polyurethane 80–95 Shore A, or hybrid with rubber

Thickness

10–30 mm; 15–20 mm typical for medium duty

Application

Troughed conveyors in coal, iron ore, copper, gold, aggregates, tailings

Service Life

6–18 months in abrasive service, depending on gap and belt speed

Benefits

Spillage containment, less belt wear, fewer stops, predictable wear allowance

 

· · ·

1. Definition: The Problem Is a Gap, Not a Belt

Spillage at a transfer point is rarely a belt problem. It is a gap problem. Material escapes through the space between the bottom of the skirtboard and the top of the belt, or around the ends where the strip stops short of the chute wall.

The fix looks trivial, and that is why it gets botched. Someone orders a roll of 150 mm strip, cuts it with a handsaw and bolts it on. Two weeks later the belt runs off-centre on one side and there is a pile of fines under the head pulley.

Custom cutting exists because a conveyor has a geometry, and the geometry varies with belt width, trough angle, idler spacing, skirtboard height, clamp bar type and the material being carried. Skirting is one component in a containment chain, so it helps to see where it sits in the wider **Conveyor** system before specifying.

· · ·

2. Three Levels of Customisation

Cut to length and width. The simplest form. Strip is cut to the skirtboard run and the required exposed height, then squared at the ends. It solves length and nothing else.

Bevel cut to trough angle. This is where most of the value sits. A 35-degree belt does not present a flat surface to the skirtboard, so the bottom edge has to be cut with a matching bevel to follow the belt profile across its full width. A straight-cut strip touches the centre idler only and leaves a wedge-shaped gap on both wings.

Fabricated assemblies. Used where the chute plan converges or diverges. Pieces are mitred and joined by vulcanised splicing or mechanical fastening to form a continuous seal. This is why **Conveyor Belt Skirting** is specified by hardness and cut tolerance together rather than by material name alone.

Polyurethane skirting profiles, installed skirt line and coiled strip ready for cutting

 

Polyurethane skirting profiles, installed skirt line and coiled strip ready for cutting

Polyurethane skirting in three forms: extruded profiles, an installed skirt line under a clamp bar, and coiled strip ready for cutting.

3. Working Principle: Why the Cut Governs the Seal

The seal is created by proximity, not pressure.

Polyurethane is stiff enough to hold a machined edge and flexible enough to deflect slightly under a loaded belt. When the skirt sits within a couple of millimetres of the belt, the belt sags between idlers under load and closes that clearance at the points that matter.

Press the skirt hard against the belt and the seal is excellent on day one, at the cost of friction, heat and cover wear. Leave a visible gap and the belt runs free, at the cost of spillage.

Three cutting decisions determine how well the compromise holds:

  • Bevel accuracy. Two degrees out across a 1200 mm belt leaves one wing floating. The seal is only as good as its worst point.
  • End treatment. Square-cut ends against a contoured chute wall leave a vertical gap. Cut to the contour, or fill the corner.
  • Edge finish. A rough cut on polyurethane leaves a ragged lower edge that picks up fines and wears unevenly.

· · ·

4. Selection Guide: What to Measure Before Ordering

Measurement

How to Take It

Why It Matters

Belt width

Face width of the belt, not the pulley

Sets the overall skirting length across the trough

Trough angle

Measured at the idler set

Determines the bevel along both wings

Skirtboard run length

Along the chute, both sides

Total linear metres and joint positions

Exposed skirt height

Clamp bar underside to belt surface

Controls flexibility and sealing force

Clamp bar profile and bolt pitch

Profile sketch plus bolt spacing

Fixes hole positions and compression

Belt line speed

m/s at normal operating rate

Fast belts need shorter skirt and tighter sealing

Material characteristics

Lump size, moisture, abrasiveness, temperature

Drives hardness and thickness

Belt construction

Plies, cover thickness, splice type

Sets how much pressure the belt tolerates

 

Two of these are routinely skipped, and both cause problems.

Belt line speed is often left off the enquiry, yet a 4 m/s belt and a 1.5 m/s belt want different skirt heights. The fast belt needs a shorter skirt so material has less chance to trap.

Splice type matters because a mechanical splice with raised fasteners will chew through skirting in weeks unless the skirt is lifted or relieved locally.

· · ·

5. Material Comparison

Property

Polyurethane

Rubber

Composite / Hybrid

Abrasion resistance

High

Moderate

High at the wear face

Cut edge stability

Holds a machined bevel

Deforms, tolerates rough cut

Depends on facing material

Conformity to imperfect belt

Moderate

High

Moderate

Compression set under clamp bar

Low

Higher

Low

Best duty

Dry, abrasive, high tonnage

Old conveyors, rough splices

High impact plus abrasion

Relative cost per metre

Higher

Lower

Highest

Procurement risk

Needs accurate dimensions

Tolerates field trimming

Needs bonding specification

 

The comparison that matters is polyurethane versus rubber. Polyurethane is harder and more dimensionally stable, so it holds a bevel cleanly and does not creep under the clamp bar. Rubber compresses more readily and tolerates a rougher cut and a less accurate belt. Neither is universally better, and the decision usually follows the condition of the belt rather than the material being carried.

· · ·

6. Application Comparison: Which Cut for Which Duty

Situation

Recommended Cut

Reason

Standard 35° trough, straight run, sound belt

Cut to length, bevelled

Lowest cost that still seals

Trough above 35°, or deep U-profile

Bevelled, checked against idler profile

Straight cut leaves wedge gaps

Tapering or converging chute

Fabricated with mitred corners

One straight piece cannot follow the plan

Mechanical splice with raised fasteners

Bevelled with relief at the splice

Otherwise the splice chews the skirt

Belt speed above 3.5 m/s

Shorter exposed height, tighter tolerance

Less time for material to trap

Badly worn or cambered belt

Rubber or hybrid, tracking corrected first

Harder edge wears the cover unevenly

 

Where impact energy is high, the belt deflects sharply at the loading point and no cut can hold a seal against that movement. Controlling deflection with an impact bed is a precondition for sealing, not an alternative to it.

· · ·

7. Industry Application Matrix

Industry

Material

Typical Issue

Skirt Specification

Coal mining

Coal, fines, damp

Dust escape at bunker discharge

15–20 mm PU, 85 Shore A, bevelled

Iron ore

Hematite or magnetite

Edge wear at chute ends

20–25 mm PU, 90 Shore A, fabricated

Copper ore

Wet, sticky ore

Bridging and carryback

15–20 mm PU, relief at splice

Gold and lithium

Fine concentrate

Loss of value in fines

Tight tolerance, 85 Shore A

Aggregates

Crushed stone, sand

Spillage on tapering chutes

Fabricated with mitred joints

Tailings

Slurry-adjacent solids

Wet material tracking

Hybrid or rubber, plus cleaner

 

Process context changes the answer. The conveyor between screening and the mill stockpile carries a high proportion of near-size material, and near-size material is what finds gaps. Downstream of filtration the product is wetter, and wet material bridges rather than flows. A skirt specified for dry crushed ore will underperform on a filter cake discharge unless moisture is stated at enquiry stage.

· · ·

8. Benefits, Applications and Selection in Six Steps

Benefits in service. A sealed skirt line keeps material inside the containment zone, which removes a cleanup task, a dust source and a housekeeping cost at the same time. It also reduces the volume of material dragged under the edge, which is the main cause of belt cover gouging. A correctly cut part leaves enough exposed height to be dropped 10 mm to 15 mm as it wears, turning a replacement into an adjustment.

Where it applies. Coal handling at bunker discharge and crusher feed; iron ore and copper transfer houses where abrasive fines cut through straight-cut strip at the ends; aggregates plants with tapering or diverging chutes; tailings-adjacent conveyors where wet material bridges any gap it finds.

  • Measure the trough angle at the idler set. Twenty, 35 and 45 degrees behave differently, and retrofitted sets often differ from the drawing.
  • Set the exposed height. Too much and the strip folds under load; too little and there is nothing left to take up as it wears.
  • Choose hardness against duty. 80–85 Shore A for general service; 90–95 Shore A where wear dominates and the belt line is true.
  • Choose thickness against impact. Thicker resists impact but is less flexible on small pulleys.
  • Decide the joint method. Vulcanised is stronger and smoother; mechanical is faster and easier to replace.
  • Confirm the belt line. Worn or mismatched idlers change where the belt actually sits.

Step six is where repeat failures originate. A plant that replaces skirting three times without measuring the idler set is buying parts to solve a geometry problem, and the geometry does not change because the part did. On **Belt Conveyors** being upgraded, reviewing the loading zone as a whole — chute, **Guide Trough**, **Heavy-Duty Conveyor Impact Bed** and **Conveyor Idlers & Rollers** together — costs less than replacing parts one at a time.

· · ·

9. Procurement Guide

A quotation request should read like a small engineering document.

What to send: belt width as face width, trough angle measured at the idler set, skirtboard run length on both sides, exposed height required, clamp bar profile and bolt pitch, belt line speed, material description with moisture and lump size, belt construction and splice type, temperature range, and a dimensioned sketch.

What to ask the supplier:

  • Can you manufacture to drawing and return a dimensioned sketch for approval?
  • Can you provide a material report stating hardness, tensile strength and tear resistance?
  • Do you support OEM replacement against existing part numbers?
  • Do you have export packing experience for long flexible sections?
  • Can you give a wear-life recommendation for this duty rather than a generic figure?

What to agree in writing: tolerance (around 2 mm on length and bevel is sensible), joint method, lead time against the shutdown window, and packing method. Long sections should be coiled or crated to prevent kinking, with the cut profile protected.

On cost. Expect one to three weeks from confirmed drawing to shipment for custom work. Judge the part on cost per month of sealed operation rather than price per metre: parts cost, plus installation labour, plus cleanup avoided, plus belt life extended, plus unplanned stops avoided. On a duty where cleanup occupies an hour per shift, the labour line alone exceeds the parts cost within months.

 

Material escaping along the skirt line at a conveyor transfer point

Material escaping along the skirt line. Spillage concentrated on one side points to a bevel or alignment problem rather than a worn skirt.

10. Failure Analysis

Problem

Possible Cause

Recommended Solution

Spillage on one side

Bevel does not match trough angle

Re-cut or re-bevel; check idler set

Spillage along full length

Skirt too high, or clamp bar loose

Lower skirt; re-torque evenly

Belt edge wear, one side

Skirt bearing on one wing, or misalignment

Reset gap; correct tracking

Worn through in weeks

Material trapped, or mechanical splice

Lift skirt at splice; review containment

Splitting at bolt holes

Over-torque, or wrong hole pitch

Re-drill to pitch; apply set torque

Cracking along bevel

Bevel too sharp, material too hard

Increase bevel radius; review hardness

Lifting at the ends

Square ends butting a contoured wall

Cut to contour, or fill corner separately

Dust rising without visible spillage

Skirt line has opened at the ends

Inspect end detail and chute contour

 

Wear through in weeks is almost always a splice problem. Uneven wear across the width is a tracking problem wearing the appearance of a material problem, and replacing the skirt without correcting tracking reproduces it on the new part within a season.

· · ·

11. Maintenance Guide

Daily. Check the skirt line at shift start. A torch along the line from the walkway is enough: look for a jet of fines, a dust plume, or buildup beneath the chute.

Weekly. Check clamp bar torque along the full run. Uneven torque is the most common cause of a skirt that seals at one end and leaks at the other.

Monthly. Measure exposed height at centre and both wings, and record it. A uniform loss of 3 mm a month is a plan; a loss of 8 mm on one wing is a bevel problem.

After any belt work. Re-check the skirt line. A skirt too tight on one side steers the belt before it visibly leaks, which makes the **Belt Tracker** the early warning instrument.

Carryback. Material adhering to the return strand builds up on idlers and pulls the belt off-line, and that misalignment can destroy a well-fitted skirt within weeks. The **Conveyor Belt Cleaner / Scraper** on the head pulley prevents the sequence at its origin.

Spares. Hold one spare cut section per transfer point. Custom parts are not available off a shelf, and a two-week lead time on a leaking point is an expensive wait.

Records. Log commissioning date, commissioning height and each monthly measurement. Sites that keep this record replace skirting on condition; sites that do not replace it on failure.

· · ·

12. Case Study

Customer type: Iron ore handling plant, northern China.

Ore type: Hematite, lump plus fines, moisture 4–6%.

Operating conditions: 1200 mm troughed belt at nominal 35 degrees, 3.2 m/s, two shifts, ambient down to −15 °C.

Problem: Spillage on the right-hand wing. Straight-cut 150 mm strip fitted three times, sealing at the centre and leaking at the wing each time. Cleanup took roughly an hour per shift.

Solution: The trough was re-measured at the idler set and found closer to 40 degrees than the 35 degrees on the drawing, because the idler set had been replaced without updating it. The strip was re-cut with a matching bevel, hole pitch corrected, exposed height set to 22 mm with 12 mm of take-up, and the gap set with the belt running loaded.

Result: Spillage stopped, cleanup dropped to a visual check, and edge wear on that side was no longer measurable over six months. The fix came from correcting a measurement, not from changing material grade.

· · ·

13. FAQ

Can polyurethane skirting be cut to any belt width?

Yes, within practical limits. Length is cut to order, so width is not the constraint. What changes is the number of pieces: belts wider than about 1800 mm are normally supplied as two or three sections joined on site.

How much gap should be left between skirting and the belt?

Contact or near-contact at the centre and both wing transitions, with no more than 2 mm to 3 mm elsewhere, set with the belt running. A larger gap leaks; a hard pre-load wears the belt cover.

Is polyurethane better than rubber?

Depends on duty. Polyurethane resists abrasion and holds its edge, suiting dry abrasive high-tonnage service. Rubber conforms to an imperfect belt and tolerates misalignment, suiting older conveyors and rough splices.

What is the most common cause of a leak?

A bevel that does not match the actual trough angle, usually because the angle was taken from a drawing rather than measured. The second cause is uneven clamp bar torque.

How long does custom work take?

One to three weeks from confirmed drawing to shipment, depending on compound availability and whether fabricated corners are involved.

Can I install without shutting down?

Not safely. The gap is set with the belt running, but access to the clamp bar needs the conveyor locked out. Most sites plan two to four hours per transfer point.

When do I replace rather than adjust?

When exposed height approaches the minimum that will seat under the clamp bar, or when the bottom edge has worn unevenly across the width.

Does skirting affect dust suppression?

Yes. A closed skirt line is the first containment stage, and anything escaping it must be compensated downstream. Where dust is the priority, the **Spray System** should be designed around a sealed loading zone.

· · ·

14. Conclusion

Custom cutting is the default answer for polyurethane skirting, not an optional extra. Three measurements decide whether the part works: the actual trough angle at the idler set, the exposed height below the clamp bar, and the clamp bar hole pitch in service.

Get those right, insist on a cut drawing before material is released, set the gap with the belt running, and leave take-up for wear.

A well-fitted skirt still cannot survive a belt being pulled off-line by carryback. On conveyors that keep losing their seal, a **Mining Secondary Belt Cleaner** where primary cleaning leaves a film is usually the missing piece.

· · ·

Related Articles

Related Products

Related Technical Guides

Related Buyer Guides

Related Comparison Articles

Contact

Annie Lu

Email: annie.lu@huataogroup.com

WhatsApp/WeChat: +86 18032422676

Website: www.tufflexscreen.com

Send the transfer point dimensions and the clamp bar profile, and we will confirm the cut specification and quote against a dimensioned drawing.Material escaping along the skirt line at a conveyor transfer point

prev
What Is the Difference Between a Gold Trommel and a Vibrating Screen?
Primary Belt Cleaner Performance: Twelve Field Checks
next
recommended for you
Get in touch with us
Product Lives
Customer service